PALLAKKI NDT EXCELLENCE CENTER PVT. LTD.
No. 411/A, 11th Cross, 4th Phase, Peenya Industrial Area,
Bangalore - 560 058 (Karnataka, India), Phone : 080-28360717, 41270949, 41147312
Mobile : +91 94480 60717, +91 94483 70954, +91 80889 38938
Email :
[email protected],
[email protected],
[email protected] TC-6677
RADIOGRAPHIC EXAMINATION REPORT
Customer : STAINLESS VESSELS FABRICATORS ULR : TC667721000024849F
No.117/D,9th 'A' Cross,Ganapathi Nagar, Report No. : PNEC/RT/21-22/N/3701 Date : 09/12/2021
3rd Phase,Peenya Indl.Area. Exam. Date : 08/12/2021
Bengaluru - 560 058. (Karnataka, India) Test Carr. Out At : Our Lab
Customer Client :
Customer DC. No.: 2352
TS RT No. : SL.No : 1283
Type of Job : Weld Zone Sensitivity : 2%
Job Description : Weld Test Coupon Source Used : X-Rays
Material : SS 304 Serial No. : X - Ray 1-XXG-2505 (250 kv)
Material Thick. : 3.73 Source Strength/KV : 150
PO No. : SVF/PO/39/2021-22 Source Size / Focal Spot : 1.5 X 1.5mm
Density Range : 2 to 4 Radiation Source : X-Rays
Exposure Tech. : DWDI
Ref. Code/Std. : ASME Sec V Art 2 Placement of IQI : Source Side
Proc. & Rev. No. : PNECPL/RT/W/01 Rev 2 Placement of Lead Symbol B : Yes
Acc. Criteria : ASME Sec IX,QW-191.1.2 IQI Type : Wire
Extent of Exam. : 100% Exposure Time : 0.4 Mim
Screen (F&B) : 0.1 mm Processing Time : 05 Min
UOM : Shim (in mm) : N/A
Reinforcement Thick. : -
Sr. Thick. RFC Optical Film
Identification SFD SOD IQI Loc. Find. Lev. Result
No. (mm) Thick. Density Size
1 Welder Name : Ramesh 3.73 - 762 - 1A06 2 to 4 5 X 4" A NSD NAP ACCEPTED
Sahani
Welder Code : SVF W-8
2 Dia 21.3 Joint : J1 3.73 - 762 - 1A06 2 to 4 5 X 4" B NSD NAP ACCEPTED
Total No. of Films :2 Film Size : 5 X 4" - 2
Total Sq. Inches : 40.00 Film Brand & Speed : Film - Agfa D7
Special Note
:
Loc. = Location , Find. = Finding, Lev. = Level, SFD = Source to Film Distance, SOD = Source to Object Distance, SSOFD = Source Side of Object to Film Distance
WELDING STANDARD DEFECTS
NSD: No Significant Defect, P: Porosity, LOF: Lack of Fusion, RT: Root Cavity, SDP: Surface Depression, LOP: Lack of Penetration,
GH: Gas Hole, BT: Burn Through, SP: Scattered Porosity, AP: Aligned Porosity, TI: Tungsten Inclusion, CP: Cluster Porosity, SI: Slag Inclusion,
SB: Suck Back, UC: Under Cut, EP: Excessive Penetration, MM: Mismatch, GW: Gas Worms, CK: Crack, NAP: Not Applicable
Notes : ● Report relates items tested only. ● Test Results are in compliance with requirements and / or specifications of technique used. ● Test Reports shall not be
reproduced except full in written approval of the Laboratory. ● If balance material is available after testing, it will be retained for 15 days maximum. ● Any complaints
about this test report should be communicated in writing within 7 Days of issue of this report.
Examined By Witnessed / Reviewed By For, Pallakki NDT Excellence Center Pvt. Ltd.
Shivakumar S Shashidhar P Pallakki Sowmya R. C
ASNT & ISNT Level III
PNEC/RT/F/03 This is Electronically generated Document, Authorised to consider without Seal. Page 1 of 1