Alccofine® 1108 KR
CEMENTITIOUS MICROFINE CRACK INJECTION GROUT
DESCRIPTION TYPICAL PROPERTIES
At 270C under laboratory conditions W/P 1:1 by
Alccofine 1108KR is highly fluid, single weight
component, cementitious pre packed micro-fine
grout powder. It is based on unique PSD Property Unit Value
technology to facilitate easy to inject and effective Dry fine
Form
filling of deep fine cracks, pores and voids. It has powder
particle size much finer than other hydraulically Component Single
setting materials like OPC. It is produced in state Particle Size
D10 micron (µ) < 2.5
of the art manufacturing plant in a controlled
D50 micron (µ) <6
environment resulting in consistent quality.
D90 micron (µ) < 12
D95 micron (µ) < 15
FIELDS OF APPLICATION
Specific Gravity - 3.0
Soil stabilization, fractured rock mass, Bulk Density Kg/m3 730±20
W/P - 0.9:1 1.54 ± 0.02
permeation grouting, curtain grouting, tunnel Wet
W/P - 1:1 Kg/Lit 1.51 ± 0.02
grouting, etc. Density
W/P - 1.1:1 1.48 ± 0.02
Joints in masonry structures, restoration of Marsh Cone Viscosity1 seconds 30 to 40
heritage structures, dams, etc. Bleeding % <3
Crack and joint repairs by injection grouting Setting Time (IS 5513 by
for RCC structures like storage silo, Vicat Apparatus)
foundation blocks, rafts, STP tanks, potable Initial hrs >1
water tanks, water bearing structures, roof, Final hrs < 12
bridges, basements, retaining walls, tunnel Compressive Strength
lining, etc. Grout (ASTM C1107-
02) MPa
3 Days >4
ADVANTAGES MPa
7 Days >7
MPa > 12
Single component, just add water, hassle free 28 Days
injection grouting 1: Orifice diameter 5 mm. Water to powder ratio by
weight shall normally be between 0.9-1.1:1 as per site
Effective penetration in and filling of deep fine condition & flow requirement. Results may vary as per
cracks, fissures & pore spaces. Imparts greater site conditions
water tightness
Compatible with structural concrete APPLICABLE STANDARDS
No specialised / costly equipment and set up
required for application IS 16993, IS 4031, IS 11578, IS 5513:1996,
Faster job execution, less turnaround time ASTM C1107-02
Environmentally friendly
Cost effective TECHNICAL SERVICE
Consult Alccofine technical service department for
the information related to the product and its
application.
Alccofine® 1108 KR
PARTICLE SIZE DISTRIBUTION CURVE
(PSD) PACKAGING
PSD is the most important property of grout
Alccofine 1108 KR is available in 25 Kg bags.
material which indicates spread / quantum of
various sizes of particles. Unique patented PSD NOTE
design ensures effective groutability of micro fine Though no additional super-plasticiser is required for
& ultrafine particles. Alccofine 1108KR, on special occasions like fast
setting or prolonged flow retention, suitable
accelerators or retarders can be used. Dosage of such
admixtures shall be ascertained after site trials.
STORAGE AND SHELF LIFE
Bags containing Alccofine 1108KR should be stored
in well-ventilated, sheltered, cool, dry area and
protected from moisture, rain and heat. Under such
storage conditions shelf life of sealed product is
minimum six months from the date of manufacture.
Need for testing of Alccofine 1108KR more than 6
month old to check conformity before its use.
HEALTH and SAFETY
MIXING PROCESS
PPE: Hand gloves, goggles and suitable respiratory
Always add powder in to water. Small quantities up mask shall be used.
to 25 kg can be mixed with hand held assembly of PRECAUTIONS: Avoid prolonged contact with
drill machine and mixing paddle with 400 to 1200 skin. Like for all other micro fine materials, may
rpm. Take 70-80% of water initially & slowly add cause irritation to eyes and respiratory system if
Alccofine 1108KR. Mix properly for 90sec & than inhaled. If swallowed seek medical attention
add remaining 20-30% water. Mix until a immediately.
smooth,lump free slurry is obtained. Larger HAZARD: Regarded as non-hazardous for
quantities shall be mixed with high speed colloidal transportation.
shear vane mixers of 1400 rpm. Mix until a smooth, DISPOSAL: Empty bags shall not be reused and
lump free slurry is obtained. To remove site disposed off as per local rules and regulations.
contaminants and lumps if any from the grout, pass it ADDITIONAL INFORMATION: Refer MSDS of
through fine sieve just prior to injection process. the product.
PRECAUTIONS
Make sure to agitate mixed grout slurry in the
container continuously. Avoid leaving mixed grout
unattended. Make sure that adequate quantity of grout
is available for continuous injection process. For
better flow & flow retention properties temperature of
water to be mixed should be less than 200C. For
vertical cracks, start injection process from bottom
most injection port. Clean all the tools and equipment
immediately after use with ample amount of water.
Alccofine® 1108 KR
DECLARATION
All the information is based on facts and figures experienced in the field and laboratory. It is the
responsibility of the end user to reconfirm the performance parameters. As company does not have any
control on handling of the product and site situation, it cannot be held responsible for deviation in the
performance parameters mentioned in this product data sheet.
CORPORATE OFFICE: MARKETING OFFICE: CONTACT:
Counto Microfine Products Pvt. Ltd. Ambuja Cements Limited, TechPort,
[email protected]Fourth Floor, Alcon House, Chalta No. ACC Thane Complex, L.B.S. Marg, www.alccofine.com
72, P.T. Sr. No. 19, Near Sai Baba Thane - 400604 +91 7030935351
Temple, Kadamba Road, Panaji – Goa,
403006
(A Joint Venture of Ambuja Cements Ltd. & Alcon )
Rev. V2/TDS/AF/1108KR/092022