TECHNICAL DATA SHEET
WEATHERBOND HI-GLOSS (formerly known as Weatherbond Flex) Updated Oct’23
Weatherbond Hi-Gloss is a premium pure acrylic-based exterior paint that offers a durable smooth
luxurious glossy finish for your exterior wall to stay glossier longer. It is specially formulated with
Quartz Technology coupled with a UV protector with superior protection performance on the
exterior wall to provide excellent colour and gloss retention.
Additionally, Colour Care Technology allows a richer and long-lasting colour appearance
Product Features:
• Luxurious glossy appearance
• Superior UV protection for longer-lasting colours and gloss retention
• Quartz Technology provides tough and hard paint film
• Excellent resistance against the effect of alkaline and efflorescence from the substrate
• Excellent protection against fungus and algae
• Excellent water resistance against visible watermark
• Superior resistance against dirt penetration from the environment
• Reduce the temperature of the selected colour range with a high SRI value
• 12 years of protection
• Green choice product
Paint Type Product Type Finishing Recommended Substrate Pack Size
Masonry, brick, plastering
1 Litre, 5 Litres, 15 Litres,
Water-based Exterior Gloss substrate and fibreboard
20 Litres
Composition
Pigment : Mainly Titanium Dioxide, functional extender, inorganic metal oxide and high-performance
organic pigment
Binder : Pure Acrylic Emulsion
Thinner : Water
Technical Data
Drying Time : Touch Dry : 30 minutes (Dependent on temperature and humidity)
: Hard Dry : 1 hour (Dependent on temperature and humidity)
Recoating Time : 2-3 hours (Dependent on temperature and humidity)
Dry Film Thickness : Around 30 m per coat
No. of Coats : 2 coats minimum
Theoretical Coverage : 10 – 12 m2 per litre per coat (Actual coverage is dependent on substrate condition, application
method, application condition and finishing appearance)
Volume Solid : ~ 39%
Shelf Life : Up to 36 months in a tightly sealed container
Application Method
Brush / Roller : Dilute the paint with not more than 5% of water. Preferably not dilute for best performance.
Recommended Coating System
Sealer / Primer : 8100 Weatherbond Sealer / 5100 Wall Sealer / 8000 Advance Wall : 1 Coat
Sealer / Expresskote Sealer / Acrylic 5170 Wall Sealer / Hi-Bond Wall
Sealer (on powdery or skim-coated surface)
Top Coat : Weatherbond Hi-Gloss : 2 Coats
P a g e 1|2
TECHNICAL DATA SHEET
Surface Preparation
Remove all loose, defective paint or powdery residues, loose chalk, dust, fungus, algae and foreign matter. Treat any areas
affected by fungus growth with Fungicidal Wash Solution. Repair cracks, and uneven surfaces with suitable exterior grade
fillers. Smoothen the filler areas with sandpaper. Surfaces to be painted must be cleaned thoroughly and dry, it must be
free from dirt, grease and other foreign matters. Allow all surfaces to dry completely prior to painting. Avoid painting
when the moisture content and alkalinity of the walls are still high. (Recommended painting specification requires the
moisture content of the walls to be below 16% measured by protimeter and the alkalinity of the walls to be below pH9.)
Spot prime with Nippon Exterior Wall Sealer.
Cleaning
Clean up equipment with water immediately after use.
Safety Precautions
• Keep container tightly closed and keep out of reach children or away from food and drink.
• Ensure good ventilation during application and drying.
• When applying paint, it is advisable to wear eye protection.
• In case of contact with eye, rinse with plenty of water immediately and seek medical advice.
• Remove splashes from skin by using soap or water.
• Paint must always be stored in a cool place.
• When transporting paint, care must be taken. Always keep container in a secure upright position.
• Dispose off any paint waste in accordance with the appropriate Environment Quality Regulations.
Note
* Theoretical Coverage is based on a mathematical formula
𝑉𝑜𝑙𝑢𝑚𝑒 𝑆𝑜𝑙𝑖𝑑 % 𝑥 10
[ ] = m2/lit/coat
𝐷𝑟𝑦 𝐹𝑖𝑙𝑚 𝑇ℎ𝑖𝑐𝑘𝑛𝑒𝑠𝑠
and does not consider LOSS FASTORS.
Variables like porosity of substrate, application method, dilution ratio, dry film thickness, opacity and so on will affect the
loss factor and can vary from 30% - 50% or even more.
The above information is given to the best of our knowledge based on laboratory tests and practical experience.
However, since we cannot anticipate or control the many conditions under which our products may be used, we can only
guarantee the quality of the product itself.
We reserve the right to alter the given without prior notice.
P a g e 2|2