0% found this document useful (0 votes)
26 views1 page

AISI329 SS2324 (F52 S32950) - X3CrNiMoN27 5 2Nr.1.4460 ENG

The document provides specifications for the stainless steel grade X3CrNiMoN27-5-2 (1.4460) according to EN 10088-3: 2014, including its chemical composition and mechanical properties. It outlines the properties for both rough turned and cold drawn conditions, detailing hardness, tensile strength, and resistance to intergranular corrosion. Additionally, it recommends working temperatures for hot forging and solution annealing processes.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
26 views1 page

AISI329 SS2324 (F52 S32950) - X3CrNiMoN27 5 2Nr.1.4460 ENG

The document provides specifications for the stainless steel grade X3CrNiMoN27-5-2 (1.4460) according to EN 10088-3: 2014, including its chemical composition and mechanical properties. It outlines the properties for both rough turned and cold drawn conditions, detailing hardness, tensile strength, and resistance to intergranular corrosion. Additionally, it recommends working temperatures for hot forging and solution annealing processes.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 1

X3CrNiMoN27-5-2 STAINLESS

Nr. 1.4460 STEELS

STANDARD REFERENCE:
EN 10088-3: 2014 (Hot-rolled and bright products)

RODACCIAI REFERENCES AND COMPARABLE STANDARDS


EUROPE ITALY GERMANY FRANCE UK USA

EN 10088-3: 2005 - - (NF A 35-574-90) (BS 1501 pt.3 -90) AISI

Grade N° Werkstoff N°
X3CrNiMoN27-5-2 1.4460 - - - Z5 CND 27 - 05 AZ - (329)

CHEMICAL COMPOSITION (CAST ANALYSIS) (%)


C / max Si / max Mn / max P / max S / max N Cr Mo Ni
0,05 1,00 2,00 0,035 0,030 0,05÷0,20 25,0÷28,0 1,30÷2,00 4,5÷6,5

MECHANICAL PROPERTIES - Rough turned (1X) in the annealed condition


Resistance to intergranular corrosion
Size max Hardness HB Rp 0,2 (MPa) Rm (MPa)** A5 (%) min** KV (J) min
(mm) max* ** min in the delivery condition in the welded condition
100 260 450 620÷880 20 85 YES YES
* Only for guidance ** The maximum HB values may be raised by 100HB or the tensile strenght value may be raised by 200 MPa and the
minimum A% value may be lowered to 20% for bars of ≤35 mm

MECHANICAL PROPERTIES - Cold drawn (2H, 2B) and ground bars (2G) in the solution annealed condition
Size max (mm) Rp 0,2 (MPa) min Rm (MPa) A5 (%) min* KV (J) min
≤ 10 610 770÷1030 12 -
> 10 ≤ 16 560 770÷1030 12 -
> 16 ≤ 40 460 620÷950 15 85
> 40 ≤ 63 460 620÷950 15 85
> 63 ≤ 100 460 620÷880 20 85
* Values valid only for size ≥5 mm

WORKING TEMPERATURES RECOMMENDED


Operation Hot forgings deformation Solution annealing (water, air)
°C 950÷1200 1020÷1100
rev. 10/2018

Mark Rodacciai Download APP

STAINLESS STEELS AISI 329 - SS2324


AUSTENITIC - FERRITIC (Duplex) (F52 – S32950)

You might also like